Finally reached a major milestone and laid out the fiberglass on the outside of the hull. I used about 40 oz of epoxy to wet out the glass, the process went fairly well and took about 2 hours. The temperature is slowly rising and it is easier to maintain 70 degrees in the shop. I did switch from 3:1 epoxy to 4:1 epoxy because of the faster cure time. With a cold shop, cure time is critical.
No pressure on this build but the South Dakota Kayak Challenge is only 52 days away!
time spent thus far, 49 hours...